Buying an Old HouseFall in love with your eyes open House life story

Book section 2.2 · page 82 · QR q10

Walls: stone, brick, lime and cracks

In the book: “How to read a crack, how to find a lime mason, photos of decayed sandstone and its repair and current links.”

Checked October 2026

Printable for book owners: Crack monitoring sheet (A4 PDF). Book owners: unlock with the code printed in your book.

In short

  • Mortar should be softer than the stone or brick: lime is meant to be the weak link.
  • Hard cement pointing traps water, so the stone wears away instead of the joint.
  • Width matters, but so does whether a crack is still moving.

Reading a crack

The lights are the book’s: ● GREEN normal, or a good sign; ▲ AMBER find out more before you commit; ■ RED stop and get a specialist to look before you go further. The colour is a starting point, not a verdict.

Crack width (BRE Digest 251)LightWhat it usually means
Up to about 1 mm● GREENUsually cosmetic.
About 1 to 5 mm▲ AMBERMay need repair; photograph it and watch it.
Over about 5 mm, tapering, stepped or growing■ REDPossible structural movement: a structural engineer.

Photograph every crack with a ruler and the date, and again in six months from the same spot.

Finding a lime mason

  • Ask to see lime work done three to five years ago or more.
  • Ask: “How will you rake out the joints, and will you use a grinder near the stone?” The right answer: by hand, and no.
  • Look for lime training (Scottish Lime Centre Trust, the Engine Shed) and trade membership, but ask about lime.

Cleaning stone

Abrasive and chemical cleaning can do permanent harm to sandstone, and often needs consent. Ask the council first. Often the right answer is not to clean at all. (The interest disclosure in the footer applies here.)

Decayed sandstone, and the repair

Close-up of a red sandstone chimney stack above a slate roof; one block has crumbled away deep behind its neighbours, with lead flashing at the base.
A block of red sandstone in a chimney stack, decayed deep behind the stones around it. Decay like this is typical where water has been trapped in the stone or the stone was laid on the wrong bed. It needs a stonemason’s view. Photo: Rory J Dench, Natural Stone Craft.
The back wall of a red sandstone cottage behind scaffolding; several stone faces above a window are covered in freshly applied red-brown repair mortar, with buckets and a hawk on the scaffold board.
Decayed sandstone faces being built back with a lime repair mortar, worked from the scaffold. Photo: Rory J Dench, Natural Stone Craft.

Coming soon: a colour photo guide to cement damage.

Official and useful links

Please read: this site is general guidance. It isn't a survey, a diagnosis, financial advice or legal advice, and it can't tell you whether a particular house is right for you. Always get independent professional advice about a specific house before you commit to buying it or to any work.